Air-Sparged Hydrocyclone for Fine Gold Flotation
The feed was conditioned with appropriate amounts of these flotation reagents in a sump for 20 minutes prior to the initiation of a test. With a collector addition of 0.08 g/kg, a promoter addition of .05 g/kg, and a frother addition of 0.1 g/kg, more than 80 percent of the gold is recovered at 2.17 opt gold.