Gravity Recoverable Gold (GRG) Test
First stage recovery attributed 10.6% of the GRG, while the second stage provided 22.8% and third stage recovery contributed 10.6% GRG at a final grind size of 76µm. The cumulative stage GRG vs. the grind size for each stage. This graph shows the liberation and gravity gold recovery characteristics for the sample. Fractional GRG for …