Refractory Gold Ore Treatment Methods
The clear solution drawn off from an agitator is run to two settling vats 16 ft. 6 in. in diameter by 4 ft. deep. The solution stands in settlers until any cloudiness has settled. It is then run through a sand filter and then to the zinc boxes. An 80 per cent gold recovery was made by the method of treatment described.